Printing Performance Evaluation of Water-dispersed Pigment Ink
according to Additive Conditions of Film Substrate Surface
Coating Agent |
Authors |
Hyeok-Jin Kim, Hye-Ji Seo, Eun-Ha Kang, Min-Woo Han1, Dong-Hyeon Lee2, Dong-Jun Kwon2, and Jin-Pyo Hong |
Institution/Affiliations |
1DYETEC, 2Gyeongsang National University |
Pages/Total page |
pp.196 ~ 205 / 10 |
Language |
Korean |
Abstract |
Water-dispersed pigment is on-going study for without air pollution in the
textile and print industry. Primer treatment is essential for the substrate to improve the
printing quality of eco-friendly water-dispersed pigment ink. Otherwise in the case of
untreated primer, the water-dispersed pigment ink will dry onto the surface and cause
defective images. This study was conducted on film substrate coating (primer) to fix
eco-friendly water-dispersed pigment ink on film substrate. The drying, bleeding, and
color strength of the pigment ink were examined depending on the composition and
mixing ratio of the coating solution. The mixing ratio of silica gel in the coating film
is increased to 0, 0.5, 1, 2 and 3 and results that DK-1-3 of silica gel ratio of 1
showed the lowest bleeding such as 52%, the letter thickness of 0.76mm and DK-1-5
of SG ratio of 3 showed the highest bleeding such as 304%, the letter thickness of
2.02mm. The mixing ratio of SPA in the coating film is increased to 2.5, 5, 7.5,
SPA ratio of 7.5 has a bleeding ratio of 9% and letter thickness of 0.544mm. It
showed the closest value to 0.5mm. According to the result, the optimal mixing ratio
of binder, polymer coagulant, silica gel is 100:7.5:1. |